Post by johnjsgems on Apr 14, 2010 17:45:54 GMT -5
Pure tin and submicron aluminum will look he same (very fine white powder). Coarser aluminum is fluffier looking (less dense) if that makes sense. Tin is reportedly the absolute best for vibe tumblers. Try it and see how it works. If her dad was old school it is more likely tin oxide. The better aluminum oxides are fairly recent products.
|
|
slabcabber
has rocks in the head
Member since April 2010
Posts: 590
|
Post by slabcabber on Apr 14, 2010 19:59:17 GMT -5
Thanks, it looks to be real fine, kinda like baby powder or even finer. I am just starting to tumble rocks, and I have a rotary tumbler will it work as good in the rotary as in the vibe?
|
|
|
Post by susand24224 on Apr 14, 2010 22:42:24 GMT -5
Yes, it will work in rotary tumblers. However, if you ever positively id it, you might want to save it for "tougher" tumbles. I have found that sometimes certain things just don't get shiny in aluminum oxide, so I then resort to cerium, or as a last resort, to tin oxide. Tin oxide costs considerably more than aluminum oxide, so you might want to hold on to at least some of it.
Susan
|
|
|
Post by johnjsgems on Apr 15, 2010 8:42:43 GMT -5
Susan, depends on what grade of aluminum oxide.
|
|
slabcabber
has rocks in the head
Member since April 2010
Posts: 590
|
Post by slabcabber on Apr 15, 2010 8:47:13 GMT -5
If I send either or both of you a sample can you tell me for sure what it is?
|
|
|
Post by johnjsgems on Apr 15, 2010 11:50:40 GMT -5
I don't think you could tell one fine white polish from another by looking. If you want to send a little I'll compare to what I have but I really don't think it would do any good. I have CPP, Titanium Dioxide, 2 grades of Al Ox, Tin Ox, and Super Cerium at home.